Acrylic vat and FEP film?


#1

Please bear with me on this.

I just picked up an old, unassembled set of moai so I am not aware of any upgrades or changes to the kit.

It has the acrylic resin vat but the peopoly store has acrylic vat and the FEP film vat.

I don’t see any mention of this on the assembly manuals or anywhere.

Can someone please enlighten me on this? So what happened? was there a change or upgrade? Do people use the acrylic ones or fep film vat?


#2

The acrylic vat with PDMS coating is the original and still standard vat. Peopoly introduced the newer, optional aluminum FEP vat this past summer.


#3

it’s fine to use the acrylic resin vat as it’s still the standard one, the FEP is optional